✓ ISO 9001 Certified Factory ✓ CE Certified / SGS Tested ✓ Ships Worldwide ✓ Free Samples Available
Get a Quote

Acrylic Sheets

Acrylic sheet is chosen for one property above all others: optical clarity. At 92% light transmission it is the clearest sheet material in common use, it holds that clarity outdoors for a decade or more, and it can be polished back to a clean edge after cutting. What it cannot do is take an impact — acrylic is brittle, and that single limitation decides most of the applications it is and is not used for.

Request a Quote Ask for Free Samples

Clear cast acrylic sheet framed as a display panel with polished edges

This page covers the cast and extruded difference, thickness selection, the comparison with polycarbonate that most buyers actually need, and the fabrication and cleaning rules that decide whether the sheet survives its first year. Grades, forming temperatures and application rules are covered in the acrylic sheet specification guide, and everything published on this range is indexed in the acrylic sheet articles.

Acrylic Sheet Specifications

Range at a glance

MaterialCast PMMA and extruded PMMA
Cast thickness1.5 – 50 mm (to 100 mm on request)
Extruded thickness1.5 – 25 mm
Sheet size2050 × 3050 mm cast; 2050 × 3050 mm extruded; cut to size
Light transmission92 % clear
Density1.19 g/cm&sup3
Service temperature−40 to +80 °C
Thermal forming150 – 180 °C
ImpactBrittle; cracks and splinters under sharp impact
Chemical resistancePoor to solvents, alcohols and ammonia — stress cracks
ColoursClear, opal, black, bronze, and 40+ standard colours
StandardEN ISO 7823 for cast and extruded PMMA sheet
Minimum order (MOQ)1 × 20GP container — mixed sizes, colours and thicknesses accepted

Cast and Extruded Acrylic Are Not the Same Sheet

Both are PMMA, both are clear, and they are sold at different prices for reasons that matter in service:

PropertyCast acrylicExtruded acrylic
Thickness range1.5 – 50 mm1.5 – 25 mm
Optical qualityBest; no orientationVery good
Thickness tolerance± 10 to 15 %± 5 %
Solvent resistanceBetterPoor; stress cracks easily
Polishing the edgePolishes back to full clarityLimited; can smear
Thermal formingSlow, needs even heatingFaster cycle
CostHigherLower
Typical useDisplays, light boxes, aquariums, furniture, signage that must lastBatch-produced signs, partitions, formed components

The practical rule: if the edge will be visible and polished, if the sheet is thick, or if it will be cleaned with anything other than soap and water, specify cast. Extruded is the right answer for volume signage and formed parts where the sheet is thin and the cost is the driver.

Thickness and What Each Range Does

  • 1.5 – 2 mm — signage faces, display covers, picture framing, machine windows.
  • 3 mm — the general-purpose display and partition thickness; light boxes, retail POS, protective covers.
  • 4 – 5 mm — larger display panels, secondary glazing, furniture fronts, sneeze guards.
  • 6 – 10 mm — aquariums, heavy display cases, illuminated signage, bar tops and furniture.
  • 12 – 25 mm — thick aquarium walls, sculptural and architectural work, machined components.
  • 30 mm and above — cast only; specialist architectural and display use.
Clear acrylic bath screen and panels installed in a bathroom

Acrylic vs Polycarbonate: The Choice That Matters

This is the comparison most buyers actually need, because the two are visually similar and behave completely differently in service:

PropertyAcrylic (PMMA)Polycarbonate (PC)
Light transmission92 %88 – 91 %
ImpactBrittle; cracks and splintersVery high; flexes and does not shatter
Scratch resistanceBetterModerate; hard coat available
Optical clarity over timeHolds for years outdoorsHolds if the UV layer is intact
Service temperature−40 to +80 °C−40 to +120 °C
FormingNeeds slow, even heatCold bends easily
Chemical resistancePoor to solvents and alcoholsPoor to alkalis and solvents
Where it belongsDisplays, light boxes, aquariums, furnitureGuards, roofing, security, machine windows

The decision is almost always about impact. Anywhere a person could fall against it, throw something at it, or where breakage is a safety issue, polycarbonate is the correct material even though acrylic looks better. Anywhere the surface is looked at rather than hit, acrylic gives the better optical result. The full comparison, including glass, is in polycarbonate glazing compared with acrylic and glass.

Fabrication, Forming and Bonding

  • Sawing and routing. Standard woodworking tools work, but the blade must be sharp and the feed steady; acrylic chips and can crack along a scribed line if forced.
  • Drilling. Use a slow speed with a brad-point bit, clear the swarf, and drill oversize — the sheet expands about 0.07 mm per metre per degree.
  • Polishing. Sand progressively then polish; cast acrylic returns to full optical clarity, extruded does not.
  • Thermal forming. 150 to 180 °C for bending and drape forming. Heat must be even or the sheet blushes and stress-cracks later.
  • Bonding. Solvent cements such as dichloromethane weld acrylic to itself; the joint is clear and strong but the solvent must be applied sparingly.
  • Annealing. Machined or formed cast acrylic benefits from annealing at about 80 °C to relieve stress — skipping this is a common cause of later crazing.

The Cleaning Rule That Saves the Sheet

Most acrylic failures we hear about are not manufacturing faults. They are cleaning damage:

  • Never use alcohol, ammonia-based glass cleaner or solvent wipes. These attack the surface and cause crazing — a network of fine cracks that appears days later and cannot be polished out.
  • Use mild neutral detergent, water and a soft cloth, then rinse and dry with another soft cloth. A dry cloth on a dusty surface scratches.
  • Never wipe a dry surface. Dust is abrasive; wipe with plenty of water.
  • Keep the protective film on until installation is finished, and remove it within the recommended period — film left in sun bakes on.

Supply, Colours and Container

  • Formats. Standard sheets plus cut-to-size, polished-edge and CNC-machined parts.
  • Colours. Clear, opal, black, bronze and a wide standard colour range; custom matching on volume.
  • Packing. Both faces filmed, interleaved, crated with edge protection. Acrylic scratches in transit more easily than polycarbonate, so the packing is not a detail.
  • Thickness tolerance. Note that cast acrylic varies ±10 to 15 % on thickness by nature; where the thickness is critical, specify extruded.

Where We Are Honest About the Limits

  • It breaks. Acrylic is brittle and, unlike polycarbonate, does not flex. Wherever impact or vandalism is a realistic risk, acrylic is the wrong specification and we will say so before quoting.
  • Solvents destroy it. Alcohol-based sanitisers, ammonia glass cleaner and solvent adhesives all cause crazing. In healthcare, food service and any environment with routine disinfectant wiping, this has to be checked before the material is chosen.
  • 80 °C is the ceiling. Acrylic softens well below polycarbonate’s range, so it is not for hot enclosures, roof glazing or anywhere near a heat source.
  • Cast thickness is not exact. ±10 to 15 % is normal for cast sheet. If a tight thickness is a functional requirement rather than a habit, extruded is the correct specification.
  • Outdoor life is good but not infinite. Acrylic resists UV far better than most plastics, but it does chalk and embrittle over long outdoor exposure, and the surface yellows slowly.

More on Acrylic Sheets

Grades, forming temperatures, annealing schedules and application rules are covered in the acrylic sheet specification guide, and everything published on this range is indexed in the acrylic sheet articles. If you are deciding between acrylic and polycarbonate for a specific job, send the application and the environment — we will tell you which one survives it.

Acrylic Sheet: Common Questions

Cast acrylic is made in moulds, has the best optical quality, holds ±10 to 15 percent thickness, resists solvents better and polishes back to full clarity. Extruded acrylic is cheaper, holds tighter thickness tolerance at ±5 percent, but stress-cracks more easily and cannot be polished back the same way.

No, the opposite. Polycarbonate resists impact without breaking while acrylic is brittle and can crack or splinter. Acrylic wins on optical clarity and scratch resistance, which is why it is used for displays rather than protective glazing.

No. Alcohol, ammonia-based cleaners and solvent wipes cause crazing, which appears as a network of fine cracks and cannot be polished out. Use mild neutral detergent with plenty of water and a soft cloth, and never wipe a dry dusty surface.

About 80 degrees C in continuous service, well below polycarbonate at 120 degrees C. It is not suitable for roof glazing, hot enclosures or anywhere near a heat source.

Solvent cements such as dichloromethane weld acrylic to itself and give a clear, strong joint. Machined and formed cast acrylic should be annealed at around 80 degrees C afterwards to relieve stress, otherwise it can craze later.

Much less than most plastics, and it holds clarity for a decade or more in normal outdoor exposure. It does still chalk and embrittle slowly over long periods, so it is not a permanent material like glass.

Send your thickness, colour and quantity for a quotation

Send us these four details and we will come back with a landed cost:

  1. Sheet type and thickness
  2. Size and quantity
  3. Application (roof / skylight / partition...)
  4. Destination country or port

Related Articles

Questions about specs or pricing? Chat with us 👋